Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D638 |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Tensile Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D638 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Tensile Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D638 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Tensile Strength | 27.58 MPa | 4000 psi | BAM 1245 |
Kraton® D1164 P (SIS) Linear Triblock Copolymer Description: Kraton D1164 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 29%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1184 K (SBS) Branched Triblock Copolymer Description: Kraton D1184 K is a clear, branched triblock copolymer based on styrene and butadiene, with a polystyrene content of 31%. It is supplied from North America in the physical form indentif.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® G1651 H (SEBS) Linear Triblock Copolymer Description: Kraton G1651 H is a clear, linear copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | >= 27.6 MPa | >= 4000 psi | ASTM D 638 |
Karina E 832-35/1-Y-ERA-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 27.6 MPa | >= 4000 psi | ASTM D 638 |
Karina E 834-35/1-Y-ERA-LMP Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 27.6 MPa | >= 4000 psi | ASTM D 638 |
Karina E 854-10/150-A-ERYB White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D638, ASTM D1709 |
Garlock 8764 PTFE Rubber Sheet Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 27.6 MPa | 4000 psi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® A1535 H (SEBS) Linear Triblock Copolymer Description: Kraton A1535 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 57%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D638, ASTM D1708 |
ScanTube PFA Tubing Information provided by ScanTube, Inc. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D412 |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D638 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
Braskem TI4020N Impact Copolymer Polypropylene Description: Extra High Izod Impact, Very Good Low Temperature Drop Impact, Good Organoleptic Properties, NucleatedApplications: Suggested Uses Include Thermoforming, Food Packaging, Dairy Container.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
Braskem TI4350P Impact Copolymer Polypropylene Description: Good balance of stiffness and impact strength, excellent organoleptic properties.Applications: Suggested uses include compounding, thin-walled injection molding.Process: Injection Moldi.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
Braskem TR3015WV2 High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Tensile Strength | 27.6 MPa | 4000 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Tensile Strength | 27.6 - 41.4 MPa | 4000 - 6000 psi | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |
|||
Tensile Strength | >= 27.6 MPa | >= 4000 psi | ASTM D 638 |
Karina E 841-08/184-A-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 27.6 MPa | 4000 psi | ASTM D412 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |
|||
Tensile Strength | >= 27.6 MPa | >= 4000 psi | ASTM D 638 |
Karina E 841-08/184-Y-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |