Material Notes:
Description: High melt flow, excellent see-through clarity, superior color and processing stability, low odor.Applications: Suggested uses include reusable food containers, housewares, fast-cycle injection molding.Process: Injection MoldingThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 31.0 MPa
4500 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256A