Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 23.0 °C |
0.900 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers OpteSTAT™ NC TPU 9020 Polyurethane-based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers C-Acetal 25GF-BK Acetal, 25% Glass Fiber Reinforced Product Description: Glass Fiber (25% Reinforced), Acetal Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristics: Pre-color.. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 23.0 °C |
0.900 ft-lb/in @Temperature 73.4 °F |
1/8'' notched bar; ASTM D256 |
Ineos H04G-00 Polypropylene Homopolymer This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications... |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.900 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ SVP6100 Nylon 610 Isocorâ„¢ 6100 is a medium viscosity PA-610. This resin is specifically suited for applications requiring low moisture absorption and greater dimensional stability. Isocorâ„¢ 6100 is also u.. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 3.17 mm |
0.900 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM HO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.481 J/cm @Temperature 22.8 °C |
0.900 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Ensinger Tecamid® 6/12 Nylon (PA612) Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256A |
Braskem TI2600C High Crystallinity Copolymer Polypropylene Description: Highly Crystalline Homopolymer Phase, Very High Molecular Weight EPR Phase, Very High Flexural Modulus, Reduced Emissions, Reduced GelsApplications: Suggested Uses Include CompoundingPr.. |
|||
Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.481 J/cm @Thickness 6.35 mm |
0.900 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 927 GHF High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |