Material Notes:
Description: Superior stiffness, good static charge dissipation, excellent mold release, nucleated.Applications: Suggested uses include closures, overcaps, cosmetic packaging, disposable cutlery.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 37.9 MPa
5500 psi
2 in/min; ASTM D638
Elongation at Yield 13.7 %
13.7 %
2 in/min; ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256A