Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Modulus | 1.86 - 11.3 GPa | 270 - 1640 ksi | Average value: 6.66 GPa Grade Count:99 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 0.1 in/min; ASTM D790 |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HI2 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Global ABS-704 General Purpose High Impact ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | |
Kraton® G1657 + PA-6,6 blend (12/8/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Spartech Royalite R84/21 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 6600 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D 790 |
Styrolution PS 5400/5401 HIPS Good ESCRHigh ImpactLow gloss (matte finish)USP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ES-0173 ABS, Extrusion Grade Extrusion ABS for the interior of refrigerator with HCFC-141b, down gauging characteristicInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4142R Injection Molding Polypropylene Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142R is a low viscosity, highly isotactic polypropylene homopolymer designed pri.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances.. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Aaron Industries AAROPRENE® CFIPP 2020 High Impact Calcium Carbonate Filled Polypropylene AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |