Breplast Bretene PP Plus Polypropylene Composite

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Breplast S.P.A.
Trade Name Bretene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Breplast Bretene PP Plus Polypropylene Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recovered polypropylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Melt Flow 28 - 32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
28 - 32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Descriptive Properties Value Comments
Color Grey