Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Mytex Polymers 1391 Polypropylene, Non-filled, Compounded Description: 1391 is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Mytex Polymers AS33L(W)-06 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L(W)-06 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and .. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Melt Flow | 28 g/10 min @Load 6.60 kg, Temperature 400 °C |
28 g/10 min @Load 14.6 lb, Temperature 752 °F |
ASTM D1238 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1492 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1492 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 250 °C |
28 g/10 min @Load 11.0 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND PCA PD 55 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Halogen free injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ). Main application fields: business machines, electroni.. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M3018-P Polyethylene
(discontinued **) Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various .. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Ineos ABS Lustran® ABS 377 Plating, Injection Molding Grade |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-9524 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9524 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9524 is dev.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® CI 31 F 000000 Copolyamide PA6/6I Copolyamide PA6/6I, low melt point (188-191°C), low viscosity, no additives, very high transparency, in compliance with FDA as far as the PA-layer is separated from the food by a 50 µm PE film.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 270 °C |
28 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 270 °C |
28 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133-1 |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 28 g/10 min | 28 g/10 min | ASTM D1238 |
Hyosung Topilene J742S PP J742S Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corpora.. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
Can be modified between 10 and 20 g/10mins; ASTM D1238 |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
JIS K7210 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 250 °C |
28 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 200 °C |
28 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 156F GPPS Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo.. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 250 °C |
28 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 250 °C |
28 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Melt Flow | 28 g/10 min @Load 1.20 kg, Temperature 300 °C |
28 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |