Buckeye Polymers BP RPP 5012 C Polypropylene, 50% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Calcium Carbonate
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 5012 C Polypropylene, 50% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packages, custom color matching, and processing additives.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Gardner Impact 14.7 J
10.8 ft-lb
ASTM D3029