Material Notes:
CEN®BX Polyimide Film are electrically conductive, and are precisely loaded with conductive fillers to produce films with tightly controlled surface resistivities. BX films provide both thermal and anti-static control and retain all the outstanding inertness, radiation and temperature resistance of other CEN®polyimide films, which make them ideal for use in extreme environments.Applications: satellite blankets, opaque cover-layers, radiant heat absorber, voice coil for loudspeaker, anti-static tapes and anti-static shielding material.All information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Thickness 46.0 - 54.0 microns
1.81 - 2.13 mil
ASTM D374
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 135 MPa
19600 psi
ASTM D882
Film Tensile Strength at Yield, TD 115 MPa
16700 psi
ASTM D882
Elongation at Yield >= 35 %
>= 35 %
ASTM D882
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Users viewing this material also viewed the following: