Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 Black Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(disconti Description/Features:Carbon Fiber ReinforcedESD ProtectionPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | <= 1.00e+7 ohm | <= 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding Information provided by PolyOne™ Corporation |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Surface Resistivity per Square | 1.00e+7 - 1.00e+12 ohm | 1.00e+7 - 1.00e+12 ohm | ASTM D257 |
Ensinger Hydel® PC-P ESD Polycarbonate (PC) HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | |
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Edgetek® MLS-XC195C-2 Polysulfone Alloy - ESD Material - Lubricated
(discontinued **) Data provided by PolyOne. |