CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRODAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material has good hot water resistance and sliding properties. Its applications include seals, scrapers and chain guides, and toothed wheels and rollers.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.17 %
0.17 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.90 %
0.90 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 200 MPa
29000 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 135 MPa
19600 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 9.20 GPa
1330 ksi
ISO 527-2
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Melting Point 166 °C
331 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
140 °C
284 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-2
Vicat Softening Point 158 °C
316 °F
VST/B/50; ISO 306
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.3

@Frequency 100 Hz
4.3

@Frequency 100 Hz
IEC 60250
4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm
1020 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0030

@Frequency 100 Hz
0.0030

@Frequency 100 Hz
IEC 60250
0.0060

@Frequency 1e+6 Hz
0.0060

@Frequency 1e+6 Hz
IEC 60250