Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name Crescent
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominantly spherical shape, and is essentially crystalline silica-free (less than 0.1%). These properties promote low abrasion to mixing and extrusion equipment while enhancing extrusion rates and overall productivity.Applications:ResinsPVCPolyolefinsPaints and CoatingsPolyurethanePuttiesRubber CompoundsMasticsPatching CompoundsTile Grouts/CaulksAdhesives and SealantsDrilling fluid/Oil field applicationsInformation provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Particle Size 16 - 24 µm
16 - 24 µm
For Median
20 µm
20 µm
Target Median Particle Size
Particle Mesh Size 200 Mesh
200 Mesh
65% passing, wet
Component Elements Properties Metric English Comments
Al2O3 0.18 %
0.18 %
Fe2O3 0.080 %
0.080 %
MgO 0.0040 %
0.0040 %
SiO2 0.20 %
0.20 %
Descriptive Properties Value Comments
Acid Solubility 98.00 Min.
CaCO3 93
Min
97.82
Typical
MgCO3 1.27