CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing

Category Polymer , Thermoset , Epoxy
Manufacturer CMT Materials
Trade Name HYTAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Excellent surface characteristics are obtained straight from machining and may be easily modified with sandpaper to carry more or less material into the mold as needed. It may be polished to a very smooth surface when necessary for working with transparent plastics.HYTAC-C1R has these outstanding attributes: 3 – 4X the toughness of epoxy-based syntactic foamGood machinabilitySuperior edge definition and detailVery low thermal conductivityExcellent material distribution Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet the specific needs. Applications: HYTAC-C1R is the first material to combine the durability of a thermoplastic syntactic with the dust free, easy machining and polishing capability of a copolymer syntactic foam. Excellent surface characteristics optimize material distribution with most plastics. Recommended for use with APET, CPET, HIPS, PETG, PLA, PP, PVC and RPET. Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.737 g/cc
0.0266 lb/in³
Mechanical Properties Metric English Comments
Flexural Toughness 0.0779 MPa
11.3 psi
ASTM D790
Compressive Strength 47.99 MPa
6960 psi
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C
35.0 µin/in-°F
Thermal Conductivity 0.130 W/m-K
0.902 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Descriptive Properties Value Comments
Color Slate Blue