Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R6000 FR-PC Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 20 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL EXT115 PPE+PS (Asia Pacific) PPE+PS, Auto exterior grade, wax remover resistant |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 40.0 - 130 °C |
35.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F123HV Color Keyed Thixotropic Epoxy Adhesive TRA-BOND F123 HV is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
Unitika M2350 PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Exce.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 3121 Rigid PVC, Extrusion Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified Information provided by Asahi Thermofil |
|||
CTE, linear | 63.0 - 310 µm/m-°C | 35.0 - 172 µin/in-°F | Average value: 214 µm/m-°C Grade Count:39 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |