CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer CMT Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling applications, providing excellent definition and dimensional stability at elevated temperatures. RenShape 472 is a moderate density, neutral-colored board with enhanced dimensional stability and excellent toughness. RenShape 472 features properties including:Ultra-fine Surface FinishHigh Flexural StrengthOutstanding Resistance to Shrinkage and WarpingTough and DurableApplications: REN 472 applications may include prototype thermoform and vacuum form molds, foundry pattens, and dimensionally stable tooling aids and fixtures.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.881 g/cc
0.0318 lb/in³
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Ultimate 48.3 MPa
7000 psi
ASTM D-638
Flexural Strength 65.8 MPa
9540 psi
ASTM D-790
Flexural Modulus 2.87 GPa
416 ksi
ASTM D-790
Compressive Strength 75.2 MPa
10900 psi
ASTM D-695
Compressive Modulus 3.17 GPa
460 ksi
ASTM D-695
Thermal Properties Metric English Comments
CTE, linear 46.4 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-3386
Glass Transition Temp, Tg 120 °C
248 °F
ASTM D-4065
Descriptive Properties Value Comments
Color Light Grey
Users viewing this material also viewed the following: