Polymer Property : Compressive Strength = 75.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 75.2 MPa
10900 psi
2% Def.; ISO 604
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet)
KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. ..
Compressive Strength 75.2 MPa
10900 psi
ASTM D-695
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures
RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling a..
Compressive Strength 75.2 MPa
10900 psi
Abatron AboCast 8103-14 One-Component Epoxy
AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting..