CMW® D58 Silver Graphite Contact Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® D58 Silver Graphite Contact Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For electrical contacts; resistant to sliding wear.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 8.67 g/cc
0.313 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 25
25
Thermal Properties Metric English Comments
Melting Point <= 980 °C
<= 1800 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Carbon, C 5.0 %
5.0 %
Silver, Ag 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000313 ohm-cm
0.00000313 ohm-cm
(55% IACS)