CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 12.27 g/cc
0.4433 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 91
91
Flexural Modulus 0.655 GPa
95.0 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 175 W/m-K
1210 BTU-in/hr-ft²-°F
Melting Point >= 980 °C
>= 1800 °F
Solidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Silver, Ag 50 %
50 %
WC 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000367 ohm-cm
0.00000367 ohm-cm
(47% IACS)
Users viewing this material also viewed the following: