C.O.I.M. FILCO® 358 Film Former for Glass Fiber Sizes

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 358 Film Former for Glass Fiber Sizes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Typical Physical and Chemical Characteristics: Filco 358 is an unsaturated polyester resin easily dispersible in water. Characteristics of the dried film:clearnon tackycompatible with unsaturated polyesters and other thermosetshighly crosslinkedlow yellowing at high temperatureinsoluble in styreneApplications: Filco 358 is suggested as a film former for continuous filament mat with low solubility.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Viscosity 1000 - 2000 cP

@Temperature 25.0 °C
1000 - 2000 cP

@Temperature 77.0 °F
MA143LFE
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
MA003LCP
Chemical Properties Metric English Comments
Acid Value 5.0 - 14
5.0 - 14
mgKOH/g, MA018LCP
Processing Properties Metric English Comments
Gel Time 6.00 - 10.0 min
6.00 - 10.0 min
MA130LFE
Descriptive Properties Value Comments
Appearance Milky Liquid