CPC - Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer CPC - Vycom Co.
Trade Name FLAMETEC™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flametec™ CP5 was formulated to meet the SEMI S93 specification for fire safety in clean room applications. CP5 meets UL 94 V-0 fire classification and is extruded for gauge and dimensional consistency. CP5 has an excellent balance of physical properties, chemical resistance and fire safety.FEATURES AND BENEFITS Fire Retardant- Meets the SEMI S93 specification and UL 94 V-0. Chemical Resistance- Resistance to a broad range of chemical processes. Color- Bright White color for any clean room or laboratory equipment. Fabrication- Cuts and welds as easy as the standard grades of PP.Impact Strength- 5 times the impact of standard PP; less breakdowns in the field. Extruded Sheet- Offers the best consistency in gauge tolerance and color.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec.; ASTM D2240
Tensile Strength, Ultimate 24.1 MPa
3500 psi
ASTM D638
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
ETL Labs