Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.931 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.931 GPa
135 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene
Data provided by Multibase.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Multibase Multi-Pro® 3011 CHI Polypropylene
Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.931 GPa
135 ksi
Tangent; ASTM D790
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black
Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus >= 0.931 GPa
>= 135 ksi
ASTM D790-79
S&E Specialty Polymers GPP1001V0M-HCO-15 PP
Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev..
Flexural Modulus 0.931 GPa
135 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 20-0202
Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 0.931 GPa
135 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790
Network Polymers NPP 25-0202 C
Description: Copolymer Polypropylene, Clarified RandomInformation provided by Network Polymers Inc.
Flexural Modulus 0.931 GPa
135 ksi
2% Secant; ASTM D 790
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e..
Flexural Modulus 0.931 GPa
135 ksi
Procedure A; ASTM D790
M. Holland Company CP503 Polypropylene Impact Copolymer
Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding
Flexural Modulus 0.931 GPa
135 ksi
1.33 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 150-1335 LMDPE Rotational Molding Resin
Description: ICORENE 150-1335 is a linear medium density polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good proce..
Flexural Modulus 0.931 GPa
135 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 195-1336 LMDPE Rotational Molding Resin
Description: ICORENE 195-1336 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti..
Flexural Modulus 0.931 GPa
135 ksi
2% Secant-Method 1; ASTM D790
Ineos HP53-25-155 HDPE
HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli..
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive)
Carbon-powder-filled, thermally stable, conductive material with consistent resistivities
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
CPC - Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP)
Flametec™ CP5 was formulated to meet the SEMI S93 specification for fire safety in clean room applications. CP5 meets UL 94 V-0 fire classification and is extruded for gauge and dimensional consist..
Flexural Modulus 0.931 GPa
135 ksi
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1
For arcing electrical contactsInformation provided by CMW Inc.
Flexural Modulus 0.931 GPa
135 ksi
CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated
For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc.
Flexural Modulus >= 0.931 GPa
>= 135 ksi
ASTM D790
Buckeye Polymers BP PPC 0210 R BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring increased impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resi..
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% Secant; ASTM D790
Amco PRIMATOP PP CO 350-40 Polypropylene Copolymer
PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013.
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem TI6350WV High Impact Copolymer Polypropylene
Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for..
Flexural Modulus 0.931 GPa
135 ksi
2% Secant-Method 1; ASTM D790
Ineos HP50-25-153 HDPE
A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)...