Cadi 15WC Tungsten Copper

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Cadi Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi 15WC Tungsten Copper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 14.25 g/cc
0.5148 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90 - 96
90 - 96
Component Elements Properties Metric English Comments
Copper, Cu 30 %
30 %
Tungsten, W 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000331 - 0.00000391 ohm-cm
0.00000331 - 0.00000391 ohm-cm
Calculated from 44-52 %IACS