Material Notes:
General DescriptionNitronic 30 is a nitrogen-strengthened austenitic stainless steel developed for applications requiring good aqueous corrosion resistance combined with good resistance to abrasive and metal-to-metal wear. Nitronic 30 has annealed mechanical properties which are well above those of typical austenitic grades such as 304. This higher strength affords the opportunity to reduce thickness at equivalent engineering loads.Galling resistance of Nitronic 30 is approximately equal to 304. It work hardens rapidly while retaining good ductility. Unlike other nitrogen-strengthened stainless steels, Nitronic 30 is subject to magnetic transformation when cold worked.Nitronic 30 exhibits outstanding corrosive wear resistance under many different sliding conditions. It is more cost effective than 409 and 304 which are typically used in wet abrasive applications.The alloy possesses good corrosion resistance in many different environments. Pitting resistance is better than 304. In sulfuric and hydrochloric acids, Nitronic 30 is superior to 409 and 410, and approaches 304 in dilute solutions.Nitronic 30 is markedly more resistant to stress corrosion cracking in hit chloride solutions at lower stress levels than 304 and 304L. At higher levels the chloride stress corrosion cracking resistance approximates 304 and 304L.ApplicationsCoal handling equipment – screens, chute liners, buckets and hopper carsWater supply and control structuresSewage treatment plant structuresMining equipment – magnetic ore separator screensBulk solids handling equipment – conveyor partsMixing tanksWear plates now using less cost effective materials such as abrasion resistance steels, 409 or 304 stainless steels.Transport and vibratory equipment where fatigue resistance is a major design criteria.Shipboard containersInformation provided by Carlson
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 241
<= 241
Hardness, Rockwell B <= 100
<= 100
Tensile Strength at Break >= 655 MPa
>= 95000 psi
Tensile Strength, Yield >= 331 MPa

@Strain 0.200 %
>= 48000 psi

@Strain 0.200 %
Elongation at Break >= 35 %
>= 35 %
Modulus of Elasticity 193 GPa
28000 ksi
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 15 - 17 %
15 - 17 %
Iron, Fe 69.6 - 76.35 %
69.6 - 76.35 %
Manganese, Mn 7.0 - 9.0 %
7.0 - 9.0 %
Nickel, Ni 1.5 - 3.0 %
1.5 - 3.0 %
Nitrogen, N 0.15 - 0.30 %
0.15 - 0.30 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Magnetic Permeability 1.011
1.011
100 Oersteds
1.014
1.014
500 Oersteds
1.015
1.015
1000 Oersteds
Users viewing this material also viewed the following: