Carmel Olefins CAPILENE® G 86 E Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® G 86 E Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAPILENE® G 86 E is a polypropylene homopolymer intended for extrusion and thermoforming applications. This grade is formulated with a low water carry-over additive packaging and it exhibits good mechanical properties and good process ability. It does not contain a slip agent or any anti-blocking agent. APPLICATIONS CAPILENE ® G 86 E is suitable for extrusion thermoforming, film extrusion (BOPP), tape extrusion for woven applications and for carpet backing. It is also a general purpose injection molding grade for technical items.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature >=23.0 °C
0.749 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525