Carmel Olefins CAPILENE® SU 75 AV Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® SU 75 AV Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® SU 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SU 75 AV is nucleated with antistatic additive. It offers outstanding processability combined with good impact strength and dimensional stability.Applications: CAPILENE® SU 75 AV is used in large items with good impact resistance such as boxes, crates, pails, thin walled containers and toys.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 44 g/10 min

@Load 2.16 kg,
Temperature 230 °C
44 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50 mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm

@Temperature -20.0 °C
0.937 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Vicat Softening Point 147 °C

@Load 1.02 kg
297 °F

@Load 2.25 lb
ASTM D1525