Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ceradyne Ceralloy® 398J Yttrium Oxide

Category Ceramic , Oxide
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® 398J Yttrium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ceralloy® 398J Hot Pressed Yttrium Oxide is a high purity hot-pressed ceramic exhibiting excellent corrosion and erosion resistance. Products produced from Hot Pressed Yttrium Oxide are for semiconductor wafer processing applicationsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 5.00 g/cc
0.181 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 585
585
0.3
Modulus of Elasticity 170 GPa
24700 ksi
Flexural Strength 99.0 MPa

@Temperature 23.0 °C
14400 psi

@Temperature 73.4 °F
Poissons Ratio 0.31
0.31
Fracture Toughness 1.40 MPa-m½
1.27 ksi-in½
Shear Modulus 64.9 GPa
9410 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature 20.0 - 1000 °C
5.06 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 14.0 W/m-K
97.2 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Descriptive Properties Value Comments
Purity, % 99.9
Users viewing this material also viewed the following: