Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: