Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N130GL (COND, 50% RH) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N130GL (COND, 50% RH) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15300 psi
ASTM D638
Flexural Strength 167 MPa
24200 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648