Chase Plastics CP Pryme® N330GL (COND, 50% RH) Nylon 6 (Utility Grade), 30% Glass Fiber Reinforced, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N330GL (COND, 50% RH) Nylon 6 (Utility Grade), 30% Glass Fiber Reinforced, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256