Chase Plastics CP Pryme® N340MGL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Mineral/Glass Fiber Reinforced, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N340MGL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Mineral/Glass Fiber Reinforced, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.1 MPa
7560 psi
ASTM D638
Flexural Strength 102.6 MPa
14880 psi
ASTM D790
Flexural Modulus 4.69 GPa
680 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256