Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 3.00 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Nylene® 453 Nylon 6, 50% RH
Injection molding grade. Nylene 453 is a UV stabilized, high viscosity nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance provided by 453 is attributed to hig..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Omni Plastics OmniTech™ HDPE GRC40 Glass Reinforced
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Omni Plastics OmniTuff™ CPP GRC30 Copolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Petromont 5000 High Density Polyethylene Resin
Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa..
Izod Impact, Notched 1.60 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM)
Information provided by Ravago.
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Elastoblend® PA6 IM 409 L MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP C..
Izod Impact, Notched 1.60 J/cm

@Thickness 6.40 mm
3.00 ft-lb/in

@Thickness 0.252 in
ASTM D256
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F, 0.125 in.; ASTM D256
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss
Information provided by Star Plastics, Inc.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Shuman 210 Polyphenylene Ether Copolymer Alloy
Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® NN100L (COND, 50% RH) Nylon 66, Internally Lubricated
Information provided by Chase Plastics.
Izod Impact, Notched 1.60 J/cm

@Temperature 23.0 °C
3.00 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek RA843 Nylon 6.6, Impact Modified
Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
A. Schulman ComAlloy® E-17036 Glass Fiber Reinforced High Heat Polycarbonate
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Ecomass® 4702ZB92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Ecomass® 4703ZB92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256A
ExxonMobil PP7505KNE2 Polypropylene Homopolymer
Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced ..
Izod Impact, Notched 1.60 J/cm

@Temperature 22.8 °C
3.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent..
Izod Impact, Notched 1.60 - 2.14 J/cm
3.00 - 4.00 ft-lb/in
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® D925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **)
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s..
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.