Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN100MD2 (DAM) Nylon 66 with 2% MoS2 Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN100MD2 (DAM) Nylon 66 with 2% MoS2 Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C
183 °F
ASTM D648
Users viewing this material also viewed the following: