Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 - 114 °C | 183 - 237 °F | Average value: 97.0 °C Grade Count:49 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
I. Stern 913 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetInformation provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0500RX Biocompatible ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0501A Antimicrobial ABS A high gloss, injection molding grade of ABS containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0502AF Food Grade ABS A high gloss, injection molding grade of ABS with FDA food contact approval, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0502ARX Biocompatible, Antimicrobial ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0505ARX Biocompatible, Antimicrobial ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
Spartech Royalstatâ„¢ R675 PS Alloy Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed; ISO 75-2/A |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | unannealed, .125in; ASTM D648 |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C @Thickness 3.17 mm |
183 °F @Thickness 0.125 in |
annealed; ASTM D648 |
Sumitomo Chemical Sumipex® LG35 Acrylic Resin, High Flow Product CharacteristicsHigh FlowImproved Cycle TimeInformation provided by Calsak Corporation |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
Chase Plastics CP Pryme® NN100MD2 (DAM) Nylon 66 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | |
Aclo Accutech ABS ABS831G10L Glass Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339W40L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339T40L1 Talc Reinforced |