Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN300L (DAM) Nylon 66 (Utility Grade), Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.86 GPa
415 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648