Material Notes:
A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 293 °C
559 °F