Polymer Property : Tensile Strength, Ultimate = 193 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 193 MPa
28000 psi
Pacific Sintered Materials FC-208-N Copper Iron Powdered Metal
Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-2000-K40All information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 193 MPa
28000 psi
PSM Industries Pacific Sintered Metals Copper Iron FC-208-N Powdered Metal
Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-2000-K40Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC  (discontinued **)
QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It of..
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Techmer ES Electrafil® J-50/CF/40 Polycarbonate, 40% Carbon Fiber Reinforced, PTFE Lubricated
Tensile Strength, Ultimate 193 MPa
28000 psi
ACMA Test #4
CoorsTek AD-94 Alumina (nom. 94% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Tensile Strength, Ultimate 193 MPa
28000 psi
annealed
CMW® ELKONIUM 217 Silver Cadmium Alloy
The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability..
Tensile Strength, Ultimate 193 MPa
28000 psi
annealed
CMW® ELKONIUM 40 pure palladium
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced
A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
Tensile Strength, Ultimate 193 MPa
28000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced  (discontinued **)
Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 193 MPa
28000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.