Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Durlex 700 PBT, General Purpose

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Chem Polymer
Trade Name Durlex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Durlex 700 PBT, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A lubricated, general purpose PBT.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Yield Strength 79.0 MPa
11500 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F
Users viewing this material also viewed the following: