Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic ML849 Flame Retardant PC

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic ML849 Flame Retardant PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm
0.0060 - 0.012 in/in
ASTM D955
Melt Index of Compound 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
ASTM D785
Tensile Strength, Yield 58.8 MPa
8530 psi
ASTM D638
Flexural Yield Strength 63.7 MPa
9250 psi
ASTM D790
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 V-0
V-0