Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON CP6062EX PC/ABS+CNT Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, .. |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | |
Microcell Composite Company CELLOMER® 6000 SBS Rubber Pellets CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY ER5001RF PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (All in One PC & Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by .. |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EN-1052 PC, FR Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® EN-1052 PC, FR Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Samyang Triloy® 215 PC/ABS alloy Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl .. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Cheng Yu Plastic ML849 Flame Retardant PC |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
Type 1; 5mm/min; ASTM D638 |
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Tensile Strength, Yield | 58.8 MPa @Thickness 3.20 mm |
8530 psi @Thickness 0.126 in |
Type 1; 5mm/min; ASTM D638 |
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 58.8 MPa | 8530 psi | ASTM D638 |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |