Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic NG1300S Nylon 66, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic NG1300S Nylon 66, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.020 cm/cm
0.0020 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 97
97
ASTM D785
Tensile Strength, Yield 157 MPa
22800 psi
ASTM D638
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Flammability, UL94 HB
HB