Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 191 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 191 MPa

@Thickness 3.20 mm
27700 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
Flexural Yield Strength 191 MPa
27700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
Flexural Yield Strength 191 MPa
27700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding.
Flexural Yield Strength 191 MPa
27700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF0079 PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF0079 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Flexural Yield Strength 191 MPa
27700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Cheng Yu Plastic NG1300S Nylon 66, 30% Glass Fiber Reinforced
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Cheng Yu Plastic T885GV3 Flame Retardant PBT, 30% Glass Fiber
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Cheng Yu Plastic T890G3 PBT, 30% Glass Fiber
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Cheng Yu Plastic FR200GV30 Flame Retardant Nylon 66, 30% Glass Fiber
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Cheng Yu Plastic FV30G25 POM, 25% Glass Fiber
Copyright © lookpolymers.com All Rights Reserved