Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic PP227 Flame Retardant Polypropylene, Medium Impact

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic PP227 Flame Retardant Polypropylene, Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 - 0.015 cm/cm
0.0070 - 0.015 in/in
ASTM D955
Melt Index of Compound 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Tensile Strength, Yield 37.3 MPa
5400 psi
ASTM D638
Flexural Yield Strength 53.9 MPa
7820 psi
ASTM D790
Izod Impact, Notched 0.412 J/cm
0.771 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 V-0
V-0