Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.412 - 0.539 J/cm | 0.772 - 1.01 ft-lb/in | Average value: 0.461 J/cm Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Izod Impact, Notched | 0.412 J/cm | 0.771 ft-lb/in | DIN 53453; ASTM D256 |
Kolon NOPLA® KE531HC PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Izod Impact, Notched | 0.412 J/cm | 0.771 ft-lb/in | DIN 53453; ASTM D256 |
Kolon NOPLA® KE911 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Izod Impact, Notched | 0.412 J/cm | 0.771 ft-lb/in | ASTM D256 |
Cheng Yu Plastic PP227 Flame Retardant Polypropylene, Medium Impact |
|||
Izod Impact, Notched | 0.412 J/cm | 0.771 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.412 J/cm | 0.771 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30G30 POM, 30% Glass Fiber |