Cheng Yu Plastic PP228H TALC 10 Polypropylene, 10% Talc, High Heat

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic PP228H TALC 10 Polypropylene, 10% Talc, High Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Melt Index of Compound 15 - 20 g/10 min
15 - 20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 101
101
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Flexural Yield Strength 49.0 MPa
7110 psi
ASTM D790
Izod Impact, Notched 0.431 J/cm
0.808 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Flammability, UL94 HB
HB