Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 0.950 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity >= 0.950 g/cc
>= 0.950 g/cc
ISO.1183 DN.53479
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Specific Gravity 0.950 - 1.45 g/cc
0.950 - 1.45 g/cc
ASTM D792
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Specific Gravity 0.950 - 0.955 g/cc
0.950 - 0.955 g/cc
ASTM D792
Ravago Manufacturing Americas Echo® RPEHDW NAT (Injection) HDPE
Available in North America Recycled Content: Yes Color: Natural Form: PelletsProcessing Method: Injection Molded Information provided by Entec
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p..
Specific Gravity 0.950 g/cc
0.950 g/cc
Method A; ASTM D792
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
LG Chemical LUTENE-H ME2500 HDPE
Description: LUTENE-H ME2500 is mainly intended for injection molding of bottle caps. It has good gas permeability characteristics and high toughness.Applications: Caps for beverage bottlesCAS No. 9..
Specific Gravity 0.950 g/cc
0.950 g/cc
LG Chemical SBR 1737 High Acrylonitrile Polymer
Description: SBR 1737 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 37% bound styrene. Raw materials for this pr..
Specific Gravity 0.950 - 0.970 g/cc
0.950 - 0.970 g/cc
Michelman® Michem® Emulsion 28640 Cationic polypropylene emulsion
Description: Cationic polypropylene emulsionUsage: Michem® Emulsion 28640 is a used as a binder and substrate coating for fibers and composites.We serve many markets through Michem® Emulsion, ..
Specific Gravity 0.950 g/cc
0.950 g/cc
UR324; STM 2
Lord Adhesives Thermosetâ„¢ UR312 / UR324 Urethane Encapsulating Gel
UR312 A/B and UR324 A/B are the same components used at different mix ratios, therefore, giving different properties.LORD UR312 and UR324 are two-component, room temperature curing urethane gels. Th..
Specific Gravity 0.950 g/cc
0.950 g/cc
STM 2
Lord Adhesives Thermosetâ„¢ UR-322 Two Component Urethane Potting Compound
Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als..
Specific Gravity 0.950 g/cc
0.950 g/cc
DIN 53479
Isoflon PEHD 300 High Density Polyethylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-1 TPE
Product Description: StarTUFF TF 75-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ XAMF-500-T Process Aid Concentrate, Concentrate Based In LLDPE
DescriptionPOLYBATCH® XAMF-500-T is a 5% active, multicomponent, process aid concentrate based in LLDPE. This concentrate is designed for use in unfilled systems to reduce/eliminate melt fracture...
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ Blue 40460/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40460/4 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 40460/4 is typically recommended..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ Blue 40460/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40460/4 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 40460/4 is typically recommended..
Specific Gravity 0.950 g/cc
0.950 g/cc
Zeon Chemicals Zetpol® 2020L Hydrogenated Nitrile Elastomomer
Zetpol 2020L is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance ..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
Specific Gravity 0.950 g/cc

@Temperature 25.0 °C
0.950 g/cc

@Temperature 77.0 °F
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane
Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792 and ISO 1183
ExxonMobil Santoprene® 121-75M200 Thermoplastic Vulcanizate - UV Resistant
Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated with high flow properties and exc..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 123-52W242 Thermoplastic Elastomer
A hard, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has low friction resistance and is especially designed for slip-coating materials in weathers..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft ..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
PolyOne Synprene® RT-3955 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved