Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic VH826 Flame Retardant ABS, Medium Impact

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic VH826 Flame Retardant ABS, Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Melt Index of Compound 5.0 - 8.0 g/10 min
5.0 - 8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 103
103
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
ASTM D638
Flexural Yield Strength 88.3 MPa
12800 psi
ASTM D790
Izod Impact, Notched 1.27 J/cm
2.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Flammability, UL94 V-2
V-2