Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.2 MPa | 5690 psi | ASTM D638 |
Hyosung Topilene B301 PP B301 HomopolymerApplications:Thermoforming sheetsCharacteristics:High melt tensionDimensional stabilityGood optical propertyInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | ASTM D638 |
Hyosung Topilene J700-1 PP J700-1 Injection Special Purpose GradeApplications:Disposable syringeHouseware applianceCharacteristics:Slip propertyHigh stiffnessFast cycleInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HG-0760AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0150AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0857 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0810 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0810 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® S168D Thermoplastic Polyurethane Type: Estane® S168D is a Shore 68D, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | ASTM D638 |
Cheng Yu Plastic VH826 Flame Retardant ABS, Medium Impact |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type 1, 5 mm/min speed; ASTM D-638 |
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa @Thickness 3.20 mm |
5690 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron SE32H Extrusion ABS Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Tensile Strength, Yield | 39.2 MPa | 5690 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |