Chesterton OPTICOOL™ 572 Lubrication

Category Fluid , Lubricant
Manufacturer Chesterton
Trade Name OPTICOOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton OPTICOOL™ 572 Lubrication.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: OPTICOOL 572 is a high performance blend of synthetic and emulsion technology OPTICOOL 572 offers superior lubrication/cooling, corrosion inhibition, extreme pressure resistance, rancidity control and hard water stability. 572 is ideal for multi-task machining center. The flexible technology and additive package arsenal allows for plant standardization of multi-machining fluids.Properties:Excellent Lubrication/Cooling PropertiesExcellent Foam ControlClean, Safe Work EnvironmentSuperior Heat DissipationExtreme Pressure CapabilityExcellent Hard Water StabilityReduces Mist and inhalation HazardsResists Microbial AttackExcellent Corrosion ProtectionMild to the SkinSuggested uses:MillingTurningGrindingStampingDrawingBroachingDrillingReamingSawingTappingTreadingInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
pH 9.0
9.0
5% Concentration
9.0 - 9.4
9.0 - 9.4
Concentrate
Viscosity Measure 22 cSt

@Temperature 40.0 °C
22 cSt

@Temperature 104 °F
Descriptive Properties Value Comments
Appearance Clear, amber
5% water
Base Semi Synthetic
Form Liquid Concentrate