Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.04 g/cc | 1.04 g/cc | 23/23°C; ASTM D792 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
LG Chemical LG704W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem.. |
|||
Specific Gravity | 1.04 - 1.06 g/cc | 1.04 - 1.06 g/cc | |
Michelman® Licomer® A 11 Acrylic polymer dispersion Licomer® A 11 is an aqueous polymer dispersion suitable for the manufacture of products for the finishing of shoes and leather. This product provides excellent gloss and flexibility, and provides.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Lucent Polymers GPP-120 Polypropylene Homopolymer, 20% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM 792 |
Multibase Multi-Flex® A 2599 TPE Thermoplastic Elastomer This material bonds to polypropylene. Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame Retardant Flexibility, GoodHeat StabilizedOzone ResistantPr.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7145-1000 TPE Product Description: StarFlex P 7145-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Europe-Africa-Middle East) Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SC 208 General Purpose Polystyrene CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a .. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle time.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Zeon Chemicals Sivic® Z2710 Polyblend Nitrile Elastomer Pre-plasticized with 70 hr DINP. Excellent for low durometer applications such as soft printing rolls. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 4020 20% Mineral-Filled Polypropylene DescriptionPolyfort® FPP 4020 is a 20% mineral-filled polypropylene designed for use when improved heat resistance and high stiffness is needed.Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | Part B |
Epoxy Technology EPO-TEK® E2001 Electrically Conductive, Silver-Filled Epoxy Product Description: EPO-TEK® E2001 is a two component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications using a snap-cure profile. Advantages & Appl.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Dow SPECTRIM™ 35-S Reaction Moldable Polymer SPECTRIM™ 35-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Aremco Ceramabind™ 880 High Temperature Inorganic Binder High Temperature, water-dispersible silicone resin for producing corrosion and moisture resistant coatings and sealing porous ceramics. Cures at 450 °F in one hour. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Aaron Industries AVPS M 100-2 Virgin Polystyrene Melt flow index may be specified. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics STYRON® 478 High Impact Polystyrene Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | DIN 53479 |
Isoflon PA 11 Polyamide 11 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | 23/23°C; ASTM D792 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |