Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips mPact™ D352 m-LLDPE Linear Low Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin provides increased modulus over most LLDPE's while retaining excellent clarity and good toughness. Applications: Industrial packagingProperty Comments: LLDPE line, 2.5:1 BUR, .08" diegap, 8" die, 56" FLH, 250 lbs/hr, 400°FData provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ASTM D1505
Melt Flow 1.0 g/10 min
1.0 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.360 GPa
52.2 ksi
at 1%; ASTM D882
Secant Modulus, TD 0.400 GPa
58.0 ksi
at 1%; ASTM D882
Coefficient of Friction, Dynamic 0.60
0.60
ASTM D1894
Coefficient of Friction, Static 0.70
0.70
ASTM D1894
Elmendorf Tear Strength MD 80 g
80 g
ASTM D1922
Elmendorf Tear Strength TD 350 g
350 g
ASTM D1922
Dart Drop Test 140 g
0.309 lb
26 in; ASTM D1709
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 68 %
68 %
45°; ASTM D2457